Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 10.5 % Show Material materials with Aluminio of 8.5 - 10.5 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Hierro | 4 - 5 % Show Material materials with Hierro of 4 - 5 % |
Manganeso | 0.8 - 2.5 % Show Material materials with Manganeso of 0.8 - 2.5 % |
Níquel | 4 - 5 % Show Material materials with Níquel of 4 - 5 % |
Otro | Rest Cu, total 1.0 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |