General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 2.5 - 3.5 % Show Material materials with Manganeso of 2.5 - 3.5 % |
Níquel | 29 - 31 % Show Material materials with Níquel of 29 - 31 % |
Otro | Rest Cu, total 0.1 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |