Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 0.2 % Show Material materials with Antimonio of 0.2 % |
Arsénico | 0.1 % Show Material materials with Arsénico of 0.1 % |
Bismuto | 5E-3 % Show Material materials with Bismuto of 5E-3 % |
Estaño | 1 % Show Material materials with Estaño of 1 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Otro | Rest Cu, total 1.0 |
Plomo | 27 - 33 % Show Material materials with Plomo of 27 - 33 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |