Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 0.35 % Show Material materials with Antimonio of 0.35 % |
Cobre | 64 - 67 % Show Material materials with Cobre of 64 - 67 % |
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 1.5 % Show Material materials with Níquel of 1.5 % |
Otro | total 0.5 |
Plomo | 4 - 6 % Show Material materials with Plomo of 4 - 6 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |