Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Antimonio | 0.3 % Show Material materials with Antimonio of 0.3 % |
Azufre | 0.1 % Show Material materials with Azufre of 0.1 % |
Estaño | 3.5 - 5 % Show Material materials with Estaño of 3.5 - 5 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 2 % Show Material materials with Níquel of 2 % |
Otro | Rest Cu, total 0.8 |
Plomo | 2 % Show Material materials with Plomo of 2 % |
Zinc | 1 - 3 % Show Material materials with Zinc of 1 - 3 % |