General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 23.0 °C | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 0.3 - 0.35 % Show Material materials with Antimonio of 0.3 - 0.35 % |
Arsénico | 0.1 - 0.15 % Show Material materials with Arsénico of 0.1 - 0.15 % |
Azufre | 0.06 - 0.1 % Show Material materials with Azufre of 0.06 - 0.1 % |
Cobre | 83.5 - 85.5 % Show Material materials with Cobre of 83.5 - 85.5 % |
Estaño | 8 - 10 % Show Material materials with Estaño of 8 - 10 % |
Fósforo | 0.03 - 0.05 % Show Material materials with Fósforo of 0.03 - 0.05 % |
Hierro | 0.25 - 0.3 % Show Material materials with Hierro of 0.25 - 0.3 % |
Manganeso | 0.1 - 0.2 % Show Material materials with Manganeso of 0.1 - 0.2 % |
Níquel | 2 % Show Material materials with Níquel of 2 % |
Otro | total 0.5,total 0.4 |
Plomo | 1.5 - 3.5 % Show Material materials with Plomo of 1.5 - 3.5 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Zinc | 3 - 5.5 % Show Material materials with Zinc of 3 - 5.5 % |