Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 - 0.25 % Show Material materials with Aluminio of 0.2 - 0.25 % |
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Cobre | 59 - 61 % Show Material materials with Cobre of 59 - 61 % |
Estaño | 0.2 - 0.25 % Show Material materials with Estaño of 0.2 - 0.25 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.15 - 0.2 % Show Material materials with Hierro of 0.15 - 0.2 % |
Manganeso | 0.15 - 0.2 % Show Material materials with Manganeso of 0.15 - 0.2 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | Rest Zn |
Plomo | 0.15 - 0.2 % Show Material materials with Plomo of 0.15 - 0.2 % |
Silicona | 0.7 - 1.1 % Show Material materials with Silicona of 0.7 - 1.1 % |