Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 100 [-] Show Material materials with Dureza Brinell of 100 [-] |
Dureza Vickers | 20.0 °C | 110 [-] Show Material materials with Dureza Vickers of 110 [-] |
Elongación | 20.0 °C | 5 % Show Material materials with Elongación of 5 % |
Elongation A100 | 20.0 °C | 3 % Show Material materials with Elongation A100 of 3 % |
Límite elástico Rp 0,2 | 20.0 °C | 330 MPa Show Material materials with Límite elástico Rp 0,2 of 330 MPa |
Resistencia a la tracción | 20.0 °C | 350 MPa Show Material materials with Resistencia a la tracción of 350 MPa |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 5.86E+7 S/m Show Material materials with Conductividad eléctrica of 5.86E+7 S/m |
Resistividad eléctrica | 20.0 °C | 1.71E-8 Ω·m Show Material materials with Resistividad eléctrica of 1.71E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Antimonio | 4E-4 % Show Material materials with Antimonio of 4E-4 % |
Arsénico | 5E-4 % Show Material materials with Arsénico of 5E-4 % |
Azufre | 1.5E-3 % Show Material materials with Azufre of 1.5E-3 % |
Bismuto | 2E-4 % Show Material materials with Bismuto of 2E-4 % |
Hierro | 1E-3 % Show Material materials with Hierro of 1E-3 % |
Otro | total 0.0065 |
Plata | 2.5E-3 % Show Material materials with Plata of 2.5E-3 % |
Plomo | 5E-4 % Show Material materials with Plomo of 5E-4 % |
Telurio | 2E-4 % Show Material materials with Telurio of 2E-4 % |