General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Dureza Vickers | 23.0 °C | 55 [-] Show Material materials with Dureza Vickers of 55 [-] | |
Elongación | 23.0 °C | 33 % Show Material materials with Elongación of 33 % | |
Límite elástico Rp 0,2 | 23.0 °C | 40 MPa Show Material materials with Límite elástico Rp 0,2 of 40 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 95 - 98 GPa Show Material materials with Módulo elástico of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Resistencia a la tracción | 23.0 °C | 200 MPa Show Material materials with Resistencia a la tracción of 200 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 20.0 °C | 1.73E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.73E-5 1/K | |
100.0 °C | 1.73E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.73E-5 1/K | ||
Conductividad térmica | 23.0 °C | 370 W/(m·K) Show Material materials with Conductividad térmica of 370 W/(m·K) | |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.20E+7 S/m Show Material materials with Conductividad eléctrica of 5.20E+7 S/m |
Resistividad eléctrica | 23.0 °C | 1.92E-8 Ω·m Show Material materials with Resistividad eléctrica of 1.92E-8 Ω·m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Brazing | soft brazing: very good | |
Workability | general (condition): very good |