General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 6.5 g/cm³ Show Material materials with Densidad of 6.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Calor específico of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Conductividad térmica | 20.0 °C | 115 W/(m·K) Show Material materials with Conductividad térmica of 115 W/(m·K) | |
Temperatura de fusión | 375 - 485 °C Show Material materials with Temperatura de fusión of 375 - 485 °C | Typical for Zinc Aluminium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.57E+7 S/m Show Material materials with Conductividad eléctrica of 1.57E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.4E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.4E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 5.4 - 6 % Show Material materials with Aluminio of 5.4 - 6 % |
Cadmio | 5E-3 % Show Material materials with Cadmio of 5E-3 % |
Cobre | 1.1 - 1.7 % Show Material materials with Cobre of 1.1 - 1.7 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Magnesio | 5E-3 % Show Material materials with Magnesio of 5E-3 % |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % |
Otro | Rest Zn |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 0.03 % Show Material materials with Silicona of 0.03 % |
Zinc | 92.18 % Show Material materials with Zinc of 92.18 % |