General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 6.3 g/cm³ Show Material materials with Densidad of 6.3 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Bending Fatigue Strength | 23.0 °C | 100 MPa Show Material materials with Bending Fatigue Strength of 100 MPa | |
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Dureza Brinell | 20.0 °C | 100 [-] Show Material materials with Dureza Brinell of 100 [-] | |
23.0 °C | 100 [-] Show Material materials with Dureza Brinell of 100 [-] | ||
Elongación A50 | 20.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | ||
Límite elástico Rp 0,2 | 20.0 °C | 220 MPa Show Material materials with Límite elástico Rp 0,2 of 220 MPa | |
23.0 °C | 220 MPa Show Material materials with Límite elástico Rp 0,2 of 220 MPa | ||
Módulo elástico | 20.0 °C | 86 GPa Show Material materials with Módulo elástico of 86 GPa | |
Resistencia a la tracción | 20.0 °C | 937 MPa Show Material materials with Resistencia a la tracción of 937 MPa | |
23.0 °C | 370 MPa Show Material materials with Resistencia a la tracción of 370 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Calor específico of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Conductividad térmica | 20.0 °C | 115 W/(m·K) Show Material materials with Conductividad térmica of 115 W/(m·K) | |
Temperatura de fusión | 375 - 485 °C Show Material materials with Temperatura de fusión of 375 - 485 °C | Typical for Zinc Aluminium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.62E+7 S/m Show Material materials with Conductividad eléctrica of 1.62E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.2E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.2E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 8 - 8.8 % Show Material materials with Aluminio of 8 - 8.8 % |
Cadmio | 6E-3 % Show Material materials with Cadmio of 6E-3 % |
Cobre | 0.8 - 1.3 % Show Material materials with Cobre of 0.8 - 1.3 % |
Estaño | 3E-3 % Show Material materials with Estaño of 3E-3 % |
Hierro | 0.06 % Show Material materials with Hierro of 0.06 % |
Magnesio | 0.02 - 0.03 % Show Material materials with Magnesio of 0.02 - 0.03 % |
Níquel | 0.02 % Show Material materials with Níquel of 0.02 % |
Otro | Rest Zn |
Plomo | 6E-3 % Show Material materials with Plomo of 6E-3 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 89.73 % Show Material materials with Zinc of 89.73 % |