General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 70 - 100 [-] Show Material materials with Dureza Brinell of 70 - 100 [-] |
Dureza Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Dureza Vickers of 75 - 105 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Elongation A100 | 20.0 °C | 20 % Show Material materials with Elongation A100 of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 110 MPa Show Material materials with Límite elástico Rp 0,2 of 110 MPa |
Módulo elástico | 20.0 °C | 143 GPa Show Material materials with Módulo elástico of 143 GPa |
Resistencia a la tracción | 20.0 °C | 300 MPa Show Material materials with Resistencia a la tracción of 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 399 J/(kg·K) Show Material materials with Calor específico of 399 J/(kg·K) |
Coeficiente de dilatación térmica | 20.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
100.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
Conductividad térmica | 20.0 °C | 59 - 120 W/(m·K) Show Material materials with Conductividad térmica of 59 - 120 W/(m·K) |
Temperatura de fusión | 1030 - 1050 °C Show Material materials with Temperatura de fusión of 1030 - 1050 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 8.00E+6 - 2.30E+7 S/m Show Material materials with Conductividad eléctrica of 8.00E+6 - 2.30E+7 S/m |
Resistividad eléctrica | 20.0 °C | 4.35E-8 - 1.25E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.35E-8 - 1.25E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 2.6 - 4.5 % Show Material materials with Níquel of 2.6 - 4.5 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.8 - 1.3 % Show Material materials with Silicona of 0.8 - 1.3 % |
Technological properties
Property | ||
---|---|---|
Brazing | soft brazing: good | |
Workability | general (condition): good |