General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 90 [-] Show Material materials with Dureza Brinell of 90 [-] | |
Dureza Vickers | 23.0 °C | 90 [-] Show Material materials with Dureza Vickers of 90 [-] | |
Elongación | 23.0 °C | 7 % Show Material materials with Elongación of 7 % | |
Elongation A100 | 23.0 °C | 3 % Show Material materials with Elongation A100 of 3 % | |
Límite elástico Rp 0,2 | 23.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 250 MPa Show Material materials with Resistencia a la tracción of 250 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Otro | Rest Cu, total 0.1 |
Plomo | 0.7 - 1.5 % Show Material materials with Plomo of 0.7 - 1.5 % |