Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 2E-3 % Show Material materials with Arsénico of 2E-3 % |
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Bismuto | 1E-3 % Show Material materials with Bismuto of 1E-3 % |
Cadmio | 0.25 - 0.4 % Show Material materials with Cadmio of 0.25 - 0.4 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Níquel | 2E-3 % Show Material materials with Níquel of 2E-3 % |
Otro | Rest Cu, total 0.30 |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Zinc | 5E-3 % Show Material materials with Zinc of 5E-3 % |