General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.6 g/cm³ Show Material materials with Densidad of 7.6 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 105 - 145 [-] Show Material materials with Dureza Brinell of 105 - 145 [-] |
Dureza Vickers | 20.0 °C | 110 - 150 [-] Show Material materials with Dureza Vickers of 110 - 150 [-] |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 210 MPa Show Material materials with Límite elástico Rp 0,2 of 210 MPa |
Resistencia a la tracción | 20.0 °C | 420 MPa Show Material materials with Resistencia a la tracción of 420 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 9 - 10 % Show Material materials with Aluminio of 9 - 10 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |