General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 80 [-] Show Material materials with Dureza Vickers of 80 [-] |
Elongación A50 | 20.0 °C | 45 % Show Material materials with Elongación A50 of 45 % |
Límite elástico Rp 0,2 | 20.0 °C | 170 MPa Show Material materials with Límite elástico Rp 0,2 of 170 MPa |
Resistencia a la tracción | 20.0 °C | 400 MPa Show Material materials with Resistencia a la tracción of 400 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 4 - 6 % Show Material materials with Aluminio of 4 - 6 % |
Estaño | 0.3 - 1.5 % Show Material materials with Estaño of 0.3 - 1.5 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Otro | Rest Cu, total 0.5 |
Zinc | 4 - 6 % Show Material materials with Zinc of 4 - 6 % |