General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Wanddicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 90 - 125 [-] Show Material materials with Dureza Vickers of 90 - 125 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa |
Resistencia a la tracción | 20.0 °C | 420 MPa Show Material materials with Resistencia a la tracción of 420 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 - 2.5 % Show Material materials with Hierro of 1.5 - 2.5 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Níquel | 29 - 32 % Show Material materials with Níquel of 29 - 32 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |