General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Dureza Brinell | 23.0 °C | 150 [-] Show Material materials with Dureza Brinell of 150 [-] | |
Dureza Vickers | 23.0 °C | 150 [-] Show Material materials with Dureza Vickers of 150 [-] | |
Elongación | 23.0 °C | 12 % Show Material materials with Elongación of 12 % | |
Elongation A100 | 23.0 °C | 8 % Show Material materials with Elongation A100 of 8 % | |
Límite elástico Rp 0,2 | 23.0 °C | 400 MPa Show Material materials with Límite elástico Rp 0,2 of 400 MPa | |
Módulo elástico | 23.0 °C | 120 - 140 GPa Show Material materials with Módulo elástico of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Resistencia a la tracción | 23.0 °C | 510 MPa Show Material materials with Resistencia a la tracción of 510 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Conductividad térmica | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Conductividad térmica of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Temperatura de fusión | 875 - 1135 °C Show Material materials with Temperatura de fusión of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Cobre | 47 - 50 % Show Material materials with Cobre of 47 - 50 % |
Otro | Rest Zn, total 0.2 |