General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.6 g/cm³ Show Material materials with Densidad of 8.6 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke,Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 80 - 130 [-] Show Material materials with Dureza Vickers of 80 - 130 [-] |
Elongación | 20.0 °C | 40 - 45 % Show Material materials with Elongación of 40 - 45 % |
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp 0,2 | 20.0 °C | 160 - 230 MPa Show Material materials with Límite elástico Rp 0,2 of 160 - 230 MPa |
Resistencia a la tracción | 20.0 °C | 360 - 480 MPa Show Material materials with Resistencia a la tracción of 360 - 480 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 61 - 64 % Show Material materials with Cobre of 61 - 64 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |