General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.7 g/cm³ Show Material materials with Densidad of 8.7 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 110 - 140 [-] Show Material materials with Dureza Vickers of 110 - 140 [-] |
Elongación A50 | 20.0 °C | 15 % Show Material materials with Elongación A50 of 15 % |
Límite elástico Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Límite elástico Rp 0,2 of 260 MPa |
Resistencia a la tracción | 20.0 °C | 380 - 470 MPa Show Material materials with Resistencia a la tracción of 380 - 470 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 60 - 63 % Show Material materials with Cobre of 60 - 63 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 11 - 13 % Show Material materials with Níquel of 11 - 13 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.5 - 1.5 % Show Material materials with Plomo of 0.5 - 1.5 % |