General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 170 [-] Show Material materials with Dureza Brinell of 170 [-] |
Dureza Vickers | 20.0 °C | 180 [-] Show Material materials with Dureza Vickers of 180 [-] |
Elongación | 20.0 °C | 5 % Show Material materials with Elongación of 5 % |
Límite elástico Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa |
Resistencia a la tracción | 20.0 °C | 650 MPa Show Material materials with Resistencia a la tracción of 650 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 42 - 45 % Show Material materials with Cobre of 42 - 45 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 4.5 - 6 % Show Material materials with Manganeso of 4.5 - 6 % |
Níquel | 11 - 13 % Show Material materials with Níquel of 11 - 13 % |
Otro | Rest Zn, total 0.2 |
Plomo | 1 - 2.5 % Show Material materials with Plomo of 1 - 2.5 % |