General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 90 - 120 [-] Show Material materials with Dureza Brinell of 90 - 120 [-] |
Dureza Vickers | 20.0 °C | 95 - 125 [-] Show Material materials with Dureza Vickers of 95 - 125 [-] |
Elongación | 20.0 °C | 45 % Show Material materials with Elongación of 45 % |
Elongation A100 | 20.0 °C | 35 % Show Material materials with Elongation A100 of 35 % |
Límite elástico Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Límite elástico Rp 0,2 of 260 MPa |
Módulo elástico | 20.0 °C | 115 GPa Show Material materials with Módulo elástico of 115 GPa |
Resistencia a la tracción | 20.0 °C | 390 MPa Show Material materials with Resistencia a la tracción of 390 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K |
300.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | |
Conductividad térmica | 20.0 °C | 58 W/(m·K) Show Material materials with Conductividad térmica of 58 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Estaño | 7.5 - 8.5 % Show Material materials with Estaño of 7.5 - 8.5 % |
Fósforo | 0.2 - 0.4 % Show Material materials with Fósforo of 0.2 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |