General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Wanddicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 125 - 160 [-] Show Material materials with Dureza Brinell of 125 - 160 [-] |
Dureza Vickers | 20.0 °C | 130 - 165 [-] Show Material materials with Dureza Vickers of 130 - 165 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 280 MPa Show Material materials with Límite elástico Rp 0,2 of 280 MPa |
Resistencia a la tracción | 20.0 °C | 460 MPa Show Material materials with Resistencia a la tracción of 460 MPa |
Chemical properties
Property | Value |
---|---|
Estaño | 7.5 - 9 % Show Material materials with Estaño of 7.5 - 9 % |
Fósforo | 0.2 - 0.4 % Show Material materials with Fósforo of 0.2 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.1 - 0.5 % Show Material materials with Plomo of 0.1 - 0.5 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |