General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.6 g/cm³ Show Material materials with Densidad of 8.6 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 85 - 115 [-] Show Material materials with Dureza Brinell of 85 - 115 [-] |
Dureza Vickers | 20.0 °C | 90 - 120 [-] Show Material materials with Dureza Vickers of 90 - 120 [-] |
Elongación | 20.0 °C | 27 % Show Material materials with Elongación of 27 % |
Elongation A100 | 20.0 °C | 20 % Show Material materials with Elongation A100 of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Límite elástico Rp 0,2 of 120 MPa |
Resistencia a la tracción | 20.0 °C | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 71 - 73 % Show Material materials with Cobre of 71 - 73 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.1 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |