General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 55 - 90 [-] Show Material materials with Dureza Vickers of 55 - 90 [-] |
Elongación | 20.0 °C | 50 % Show Material materials with Elongación of 50 % |
Elongación A50 | 20.0 °C | 40 % Show Material materials with Elongación A50 of 40 % |
Límite elástico Rp 0,2 | 20.0 °C | 170 MPa Show Material materials with Límite elástico Rp 0,2 of 170 MPa |
Resistencia a la tracción | 20.0 °C | 280 - 380 MPa Show Material materials with Resistencia a la tracción of 280 - 380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 66 - 68 % Show Material materials with Cobre of 66 - 68 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.1 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |