General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 80 [-] Show Material materials with Dureza Brinell of 80 [-] |
Dureza Vickers | 23.0 °C | 85 [-] Show Material materials with Dureza Vickers of 85 [-] |
Elongación | 23.0 °C | 15 - 20 % Show Material materials with Elongación of 15 - 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 120 - 140 MPa Show Material materials with Límite elástico Rp 0,2 of 120 - 140 MPa |
Resistencia a la tracción | 23.0 °C | 350 - 360 MPa Show Material materials with Resistencia a la tracción of 350 - 360 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Cobre | 57 - 59 % Show Material materials with Cobre of 57 - 59 % |
Estaño | 0.2 - 0.5 % Show Material materials with Estaño of 0.2 - 0.5 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Rest Zn, total 0.2 |
Plomo | 1.6 - 2.5 % Show Material materials with Plomo of 1.6 - 2.5 % |