General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Wanddicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 60 - 80 [-] Show Material materials with Dureza Brinell of 60 - 80 [-] |
Dureza Vickers | 20.0 °C | 65 - 85 [-] Show Material materials with Dureza Vickers of 65 - 85 [-] |
Elongación | 20.0 °C | 50 % Show Material materials with Elongación of 50 % |
Límite elástico Rp 0,2 | 20.0 °C | 115 MPa Show Material materials with Límite elástico Rp 0,2 of 115 MPa |
Resistencia a la tracción | 20.0 °C | 380 MPa Show Material materials with Resistencia a la tracción of 380 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 81 - 84 % Show Material materials with Cobre of 81 - 84 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.8 - 1.4 % Show Material materials with Níquel of 0.8 - 1.4 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.8 - 1.3 % Show Material materials with Silicona of 0.8 - 1.3 % |