General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dicke |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 70 - 105 [-] Show Material materials with Dureza Vickers of 70 - 105 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 90 MPa Show Material materials with Límite elástico Rp 0,2 of 90 MPa |
Resistencia a la tracción | 20.0 °C | 330 MPa Show Material materials with Resistencia a la tracción of 330 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.8 - 2.3 % Show Material materials with Aluminio of 1.8 - 2.3 % |
Arsénico | 0.02 - 0.06 % Show Material materials with Arsénico of 0.02 - 0.06 % |
Cobre | 76 - 79 % Show Material materials with Cobre of 76 - 79 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.07 % Show Material materials with Hierro of 0.07 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |