Chemical properties
Property | Value |
---|---|
Aluminio | 1.8 - 2.3 % Show Material materials with Aluminio of 1.8 - 2.3 % |
Arsénico | 0.02 - 0.035 % Show Material materials with Arsénico of 0.02 - 0.035 % |
Cobre | 76 - 79 % Show Material materials with Cobre of 76 - 79 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.07 % Show Material materials with Hierro of 0.07 % |
Magnesio | 5E-3 % Show Material materials with Magnesio of 5E-3 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Otro | Rest Zn, total 0.1 |
Plomo | 0.07 % Show Material materials with Plomo of 0.07 % |