General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 190 [-] Show Material materials with Dureza Brinell of 190 [-] |
Dureza Vickers | 20.0 °C | 200 [-] Show Material materials with Dureza Vickers of 200 [-] |
Elongación | 20.0 °C | 8 % Show Material materials with Elongación of 8 % |
Límite elástico Rp 0,2 | 20.0 °C | 540 MPa Show Material materials with Límite elástico Rp 0,2 of 540 MPa |
Resistencia a la tracción | 20.0 °C | 780 MPa Show Material materials with Resistencia a la tracción of 780 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 5 - 6 % Show Material materials with Aluminio of 5 - 6 % |
Cobre | 63 - 65 % Show Material materials with Cobre of 63 - 65 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 2 - 3.5 % Show Material materials with Hierro of 2 - 3.5 % |
Manganeso | 3.5 - 5 % Show Material materials with Manganeso of 3.5 - 5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |