General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 170 - 200 [-] Show Material materials with Dureza Brinell of 170 - 200 [-] |
Dureza Vickers | 20.0 °C | 180 - 210 [-] Show Material materials with Dureza Vickers of 180 - 210 [-] |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico Rp 0,2 | 20.0 °C | 360 MPa Show Material materials with Límite elástico Rp 0,2 of 360 MPa |
Resistencia a la tracción | 20.0 °C | 620 MPa Show Material materials with Resistencia a la tracción of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 4 - 5 % Show Material materials with Aluminio of 4 - 5 % |
Cobre | 65 - 68 % Show Material materials with Cobre of 65 - 68 % |
Estaño | 0.9 - 1.3 % Show Material materials with Estaño of 0.9 - 1.3 % |
Hierro | 0.5 - 3 % Show Material materials with Hierro of 0.5 - 3 % |
Manganeso | 0.5 - 3 % Show Material materials with Manganeso of 0.5 - 3 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |