General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 115 - 145 [-] Show Material materials with Dureza Brinell of 115 - 145 [-] |
Dureza Vickers | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Vickers of 120 - 150 [-] |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa |
Módulo elástico | 20.0 °C | 108 GPa Show Material materials with Módulo elástico of 108 GPa |
Resistencia a la tracción | 20.0 °C | 460 MPa Show Material materials with Resistencia a la tracción of 460 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.92E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.92E-5 1/K |
100.0 °C | 1.92E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.92E-5 1/K | |
Conductividad térmica | 20.0 °C | 71 W/(m·K) Show Material materials with Conductividad térmica of 71 W/(m·K) |
Temperatura de fusión | 880 - 915 °C Show Material materials with Temperatura de fusión of 880 - 915 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 8.90E+6 S/m Show Material materials with Conductividad eléctrica of 8.90E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.12E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.12E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 66 - 70 % Show Material materials with Cobre of 66 - 70 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.8 % Show Material materials with Plomo of 0.8 % |
Silicona | 0.7 - 1.3 % Show Material materials with Silicona of 0.7 - 1.3 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : medium, soft brazing: medium | |
Workability | Cold forming degree between anneals: max. 80 %, general (condition): good |