General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 80 - 120 [-] Show Material materials with Dureza Brinell of 80 - 120 [-] |
Dureza Vickers | 20.0 °C | 85 - 125 [-] Show Material materials with Dureza Vickers of 85 - 125 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 170 MPa Show Material materials with Límite elástico Rp 0,2 of 170 MPa |
Resistencia a la tracción | 20.0 °C | 340 MPa Show Material materials with Resistencia a la tracción of 340 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 61 - 63 % Show Material materials with Cobre of 61 - 63 % |
Estaño | 1 - 1.5 % Show Material materials with Estaño of 1 - 1.5 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.2 - 0.6 % Show Material materials with Plomo of 0.2 - 0.6 % |