General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 100 [-] Show Material materials with Dureza Brinell of 100 [-] |
Dureza Vickers | 20.0 °C | 105 [-] Show Material materials with Dureza Vickers of 105 [-] |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa |
Resistencia a la tracción | 20.0 °C | 440 MPa Show Material materials with Resistencia a la tracción of 440 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 1.3 % Show Material materials with Aluminio of 0.3 - 1.3 % |
Cobre | 57 - 59 % Show Material materials with Cobre of 57 - 59 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.8 - 1.8 % Show Material materials with Manganeso of 0.8 - 1.8 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |
Silicona | 0.2 - 0.8 % Show Material materials with Silicona of 0.2 - 0.8 % |