Chemical properties
Property | Value |
---|---|
Aluminio | 0.6 % Show Material materials with Aluminio of 0.6 % |
Cobre | 56 - 59 % Show Material materials with Cobre of 56 - 59 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.5 - 1.8 % Show Material materials with Manganeso of 0.5 - 1.8 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.7 - 1.8 % Show Material materials with Plomo of 0.7 - 1.8 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |