General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 110 - 140 [-] Show Material materials with Dureza Brinell of 110 - 140 [-] |
Dureza Vickers | 20.0 °C | 115 - 145 [-] Show Material materials with Dureza Vickers of 115 - 145 [-] |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 270 MPa Show Material materials with Límite elástico Rp 0,2 of 270 MPa |
Resistencia a la tracción | 20.0 °C | 460 MPa Show Material materials with Resistencia a la tracción of 460 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Cobre | 56.5 - 58.5 % Show Material materials with Cobre of 56.5 - 58.5 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Manganeso | 1 - 2 % Show Material materials with Manganeso of 1 - 2 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Otro | Rest Zn, total 0.4 |
Plomo | 0.5 % Show Material materials with Plomo of 0.5 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |