Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 0.1 % Show Material materials with Azufre of 0.1 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Estaño | 9.5 - 10.5 % Show Material materials with Estaño of 9.5 - 10.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Cu, total 0.50 |
Plomo | 1.5 % Show Material materials with Plomo of 1.5 % |
Silicona | 0.02 % Show Material materials with Silicona of 0.02 % |
Zinc | 1.75 - 2.75 % Show Material materials with Zinc of 1.75 - 2.75 % |