Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 1.5 % Show Material materials with Aluminio of 0.5 - 1.5 % |
Cobre | 55 - 60 % Show Material materials with Cobre of 55 - 60 % |
Estaño | 1 % Show Material materials with Estaño of 1 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Manganeso | 0.1 - 1.5 % Show Material materials with Manganeso of 0.1 - 1.5 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Plomo | 0.4 % Show Material materials with Plomo of 0.4 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 33 - 42 % Show Material materials with Zinc of 33 - 42 % |