Chemical properties
Property | Value |
---|---|
Aluminio | 3 - 5 % Show Material materials with Aluminio of 3 - 5 % |
Cobre | 60 - 65 % Show Material materials with Cobre of 60 - 65 % |
Estaño | 0.5 % Show Material materials with Estaño of 0.5 % |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % |
Manganeso | 2.5 - 5 % Show Material materials with Manganeso of 2.5 - 5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 22 - 28 % Show Material materials with Zinc of 22 - 28 % |