Chemical properties
Property | Value |
---|---|
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Cobre | 64 - 67 % Show Material materials with Cobre of 64 - 67 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Níquel | 5 - 6.5 % Show Material materials with Níquel of 5 - 6.5 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |