Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Bismuto | 3E-3 % Show Material materials with Bismuto of 3E-3 % |
Cobre | 79 - 81 % Show Material materials with Cobre of 79 - 81 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Otro | Rest Zn, total 1.5 |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Silicona | 2.5 - 4 % Show Material materials with Silicona of 2.5 - 4 % |