Chemical properties
Property | Value |
---|---|
Aluminio | 1.75 - 2.5 % Show Material materials with Aluminio of 1.75 - 2.5 % |
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Cobre | 76 - 79 % Show Material materials with Cobre of 76 - 79 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.07 % Show Material materials with Hierro of 0.07 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.07 % Show Material materials with Plomo of 0.07 % |