Chemical properties
Property | Value |
---|---|
Aluminio | 2.5 - 3.5 % Show Material materials with Aluminio of 2.5 - 3.5 % |
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 3E-3 % Show Material materials with Bismuto of 3E-3 % |
Cobre | 57 - 60 % Show Material materials with Cobre of 57 - 60 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Níquel | 2 - 3 % Show Material materials with Níquel of 2 - 3 % |
Otro | Rest Zn, total 0.9 |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |