Chemical properties
Property | Value |
---|---|
Aluminio | 1.6 - 2.2 % Show Material materials with Aluminio of 1.6 - 2.2 % |
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Cobre | 73 - 76 % Show Material materials with Cobre of 73 - 76 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Manganeso | 0.3 - 0.7 % Show Material materials with Manganeso of 0.3 - 0.7 % |
Níquel | 2 - 3 % Show Material materials with Níquel of 2 - 3 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.3 - 0.7 % Show Material materials with Silicona of 0.3 - 0.7 % |