Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.5 % Show Material materials with Antimonio of 0.5 % |
Cobre | 70 - 76 % Show Material materials with Cobre of 70 - 76 % |
Estaño | 6 - 9 % Show Material materials with Estaño of 6 - 9 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Plomo | 16 - 22 % Show Material materials with Plomo of 16 - 22 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |