Chemical properties
Property | Value |
---|---|
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Cobre | 59 - 61 % Show Material materials with Cobre of 59 - 61 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Otro | Rest Zn, total 0.5 |
Plomo | 0.6 - 1 % Show Material materials with Plomo of 0.6 - 1 % |