Chemical properties
Property | Value |
---|---|
Antimonio | 1E-3 % Show Material materials with Antimonio of 1E-3 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Azufre | 2E-3 % Show Material materials with Azufre of 2E-3 % |
Bismuto | 5E-4 % Show Material materials with Bismuto of 5E-4 % |
Estaño | 1E-3 % Show Material materials with Estaño of 1E-3 % |
Fósforo | 1E-3 % Show Material materials with Fósforo of 1E-3 % |
Hierro | 1E-3 % Show Material materials with Hierro of 1E-3 % |
Níquel | 1E-3 % Show Material materials with Níquel of 1E-3 % |
Otro | Cu+Ag > 99.97 |
Oxígeno | 0.02 % Show Material materials with Oxígeno of 0.02 % |
Plata | 2E-3 % Show Material materials with Plata of 2E-3 % |
Plomo | 2E-3 % Show Material materials with Plomo of 2E-3 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |