Chemical properties
Property | Value |
---|---|
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 2E-3 % Show Material materials with Arsénico of 2E-3 % |
Azufre | 4E-3 % Show Material materials with Azufre of 4E-3 % |
Bismuto | 1E-3 % Show Material materials with Bismuto of 1E-3 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Hierro | 4E-3 % Show Material materials with Hierro of 4E-3 % |
Níquel | 2E-3 % Show Material materials with Níquel of 2E-3 % |
Otro | Cu+Ag > 99.95 |
Plomo | 4E-3 % Show Material materials with Plomo of 4E-3 % |
Zinc | 3E-3 % Show Material materials with Zinc of 3E-3 % |