Chemical properties
Property | Value |
---|---|
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Arsénico | 0.01 % Show Material materials with Arsénico of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Bismuto | 3E-3 % Show Material materials with Bismuto of 3E-3 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | Cu+Ag > 99.50 |
Oxígeno | 0.08 % Show Material materials with Oxígeno of 0.08 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |