Chemical properties
Property | Value |
---|---|
Antimonio | 5E-3 % Show Material materials with Antimonio of 5E-3 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Cobre | 62 - 64 % Show Material materials with Cobre of 62 - 64 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.5 - 0.8 % Show Material materials with Níquel of 0.5 - 0.8 % |
Otro | Rest Zn, total 0.3 |
Plomo | 0.8 - 1.2 % Show Material materials with Plomo of 0.8 - 1.2 % |